Cr Self-Diffusion Askill 1971
(2013-07-08)
Self diffusion of Cr-51 in pure chromium, Cr +20 wt% Ni, Cr +44wt% Ni, and Cr +65%wt Ni has been measured over the temperature ranges of 1000 to 1900, 1000 to 1525, and 900 to 1350 degrees C, respectively.