Browsing CALPHAD Assessments by Subject "Co superalloys"
Now showing items 1-1 of 1
-
Development of a Diffusion Mobility Database for Co-based Superalloys
To facilitate the development of high-temperature Co-based gamma-gamma prime superalloys, a Co-Ni based diffusion mobility database is developed for the eight component FCC (Face Centered Cubic) system of Co-Al-W-Ni-Cr-Ti-Ta-Re. ...